Jan 31, 2002 #1 Shibuz Chemical Joined Apr 12, 2001 Messages 13 Location US I do have the following results when we did an x-ray diffraction on a down hole sample. Quartz (SlO2) Trace Calcite (CaCO3) Trace Barite (BaSO4) Trace Mackinawite (FeSO9) 70% Troilite ( FeS) 30% What do I make out of it? Please educate...
I do have the following results when we did an x-ray diffraction on a down hole sample. Quartz (SlO2) Trace Calcite (CaCO3) Trace Barite (BaSO4) Trace Mackinawite (FeSO9) 70% Troilite ( FeS) 30% What do I make out of it? Please educate...
Mar 10, 2003 #2 mudanimal Petroleum Joined Jun 16, 2000 Messages 3 Location US It would appear that this could be a reaction of H2S with Iron. Upvote 0 Downvote