I have a subcontractor that installed 6x6 - W1.4xW1.4 welded wire fabric instead of the 6x6 – W6xW6. This does not meet the temperature and shrikage requirements of ACI 318.
The owner is concerned that his concrete will crack because of this error. the slab measures 6 inch deep on 1 foot of gravel, and is 20' x 20'. with all the piping installed. There is no structural loading concern as it will be used to store misc. lightweight equipment.
I recommended an epoxy coating on top, however the owner feels that this is still not what he paid for so he wants to demo (remove) and reinstall with the correct size wire.
Is this excessive or needed?
The owner is concerned that his concrete will crack because of this error. the slab measures 6 inch deep on 1 foot of gravel, and is 20' x 20'. with all the piping installed. There is no structural loading concern as it will be used to store misc. lightweight equipment.
I recommended an epoxy coating on top, however the owner feels that this is still not what he paid for so he wants to demo (remove) and reinstall with the correct size wire.
Is this excessive or needed?