Hi everybody,
Question is determination of WPS thickness range.
PQR
Pipe type: A 333 Gr6
Thickness T: 3.76 mm
Impact test requirement: YES according to design code ASME B31.3
Welding Process: GTAW
----------------------------------
So, the WPS min/max thickness range qualified shall be?
1. According ASME B31.3 Table 323.3.1
t/2 to t+6mm?
1.88 (3.76 /2) mm to 9.76 (3.76 + 6)mm
or
2. According to ASME Section IX QW 403.6 and QW-451.1?
QW-403.6 - “However, where T is 1/4 in. (6 mm) or less, the minimum thickness qualified is 1/2T”
QW-451.1 - 1.5 to 2T
1.88 (3.76 /2) mm to 7.52 (3.76 x 2)mm
or
3. Another range
Please, help with your response and explanation.
Thanks in advance.
Question is determination of WPS thickness range.
PQR
Pipe type: A 333 Gr6
Thickness T: 3.76 mm
Impact test requirement: YES according to design code ASME B31.3
Welding Process: GTAW
----------------------------------
So, the WPS min/max thickness range qualified shall be?
1. According ASME B31.3 Table 323.3.1
t/2 to t+6mm?
1.88 (3.76 /2) mm to 9.76 (3.76 + 6)mm
or
2. According to ASME Section IX QW 403.6 and QW-451.1?
QW-403.6 - “However, where T is 1/4 in. (6 mm) or less, the minimum thickness qualified is 1/2T”
QW-451.1 - 1.5 to 2T
1.88 (3.76 /2) mm to 7.52 (3.76 x 2)mm
or
3. Another range
Please, help with your response and explanation.
Thanks in advance.