JohnTM
Mechanical
- Jan 24, 2004
- 8
I need to perform a PQR on a listed base material being welded to an unlisted, forged and heat treated material. I should be using Figure 4.19 from D1.1:2010, the fillet weld soundness test.
The problem is, with the forged material, I cannot make or buy a plate that matches the dimensions shown in Fig 4.19, .5" x 6.00" x 12.00".
The forged material is not pipe, it is solid, round material. That said, I could reproduce Figure 4.20, detail B, the pipe to plate fillet weld soundness test with what I have, except the round material is not 3" tall it is only 1/2" tall. Is that a possible avenue?
Are there ways of producing a qualified WPS when you can't actually weld a Figure 4.19 test?
Thanks in advance for any help.
The problem is, with the forged material, I cannot make or buy a plate that matches the dimensions shown in Fig 4.19, .5" x 6.00" x 12.00".
The forged material is not pipe, it is solid, round material. That said, I could reproduce Figure 4.20, detail B, the pipe to plate fillet weld soundness test with what I have, except the round material is not 3" tall it is only 1/2" tall. Is that a possible avenue?
Are there ways of producing a qualified WPS when you can't actually weld a Figure 4.19 test?
Thanks in advance for any help.