Apr 21, 2012 #1 kkp3456 Petroleum Joined May 14, 2011 Messages 10 Location SA Usually the WPS made is considering the piping design. So is there any specific WPS for welding of tubes or do we apply the same rules for tubes as we do in for pipes?
Usually the WPS made is considering the piping design. So is there any specific WPS for welding of tubes or do we apply the same rules for tubes as we do in for pipes?
Apr 21, 2012 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US A single WPS can be developed for both tubing and piping under ASME Section IX. Upvote 0 Downvote
Apr 21, 2012 #3 gtaw Structural Joined Feb 10, 2006 Messages 1,988 Location US A single WPS can be developed to weld structural shapes, pipe, or tubing. Best regards - Al Upvote 0 Downvote