Dear friends,
I have sumitted WPS for pipeline welding which covers thicknes 4.6 to 19.1mm.But client demand me to submit separate WPS for Hot induction bend pipe joint.the bend pipes also comes under 4.6-19.1 mm thickness,material is also same.It required to submit new WPS?
Please explain
 
ASME B31.1 and B31.3 do not require qualification on hot induction bends. Your Client is free to specify the additional testing; however, if he has changed the Contract, you have added charges to apply to him.
 
Mr.weldstan
My job is API 1104 pipeline welding is it applicable.
 
Is it because the applicable specification is classing heat treatment condition, or possibly pipe supplier, as an essential variable?

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top