Wood Beams in Torsion 1

Status
Not open for further replies.

JSA

Structural
May 28, 2001
24
Does anyone have a reference for designing a wood beam for torsion. I took a quick look in Breyer's book and didn't see anything.
 
Replies continue below

Recommended for you

I ran into this problem once before, asked around the office and my professor from my Timber Design class. They all told me to avoid it. I'd be interested to hear if anybody has any good suggestions on how.
 
I suspect the torsional strength is too low and unreliable for timber torsion design to be worthwhile.
Timber's natural tendency to split along the grain will be exacerbated by torsion.
 
Also, I used the equation and got 530 psi for my application. Back to the drawing board......

Thank you for your responses.
 
The aitc timber designers handbook has some info on this.

I dont have a copy, but I recall that it basically follows classic torsion theory for a solid rectangle and compares the shear and acial stress values to the allowable.
 