Hello, sorry I saw the question only now. In what equipment (brand and model) you are testing? Are you manually calculating the Ts1 and Ts2 or the software is giving this?
In the Alpha (previously Monsanto) ODR and MDR, when equiped with a colection system, it will always have the data points, but maybe your system is not configurate to show it. For instance, in our company, we normally use Ts1, but our sister plants in France uses the Ts2... when we want to compare some compounds, it is just matter of using the data existent...
If you have any question regarding rheometer in rubber, please let me know we I'll be glad to help.
Daniel.