We have Custom 465 parts heat treated to H-950. Then wire EDM cut in few places. When loaded the part break into many pieces, in a very brittle fracture. We suspect hydrogen embrittlement although there whs no checmical cleaning, pickling, or passivation. After baking another part in an oven for 24 hours the part was tested and found to be OK. Is it possible that the EDM procces produced hydrogen that penetrated the base metal.
Any article or reference will be appreciated.