I know some of you guys have a lot of experience when it comes to manufacturing gears and splines. I am looking to get a little help/input on manufacturing an internal involute spline.
To produce the internal spline we plan to use a wire EDM as we do not have the proper equipment to broach it. My fear with using a wire EDM is the re-cast layer that it produces. The adapter is going to be made from nitralloy and the teeth will be nitrided. So I am concerned that the re-cast layer may produce a brittle layer that when nitrided becomes even more brittle. Is it possible to remove this re-cast layer through hand lapping with a male plug?
I was hoping someone with experience could shed some more light on the issue and possible ways of getting around it.
Thank you
I know some of you guys have a lot of experience when it comes to manufacturing gears and splines. I am looking to get a little help/input on manufacturing an internal involute spline.
To produce the internal spline we plan to use a wire EDM as we do not have the proper equipment to broach it. My fear with using a wire EDM is the re-cast layer that it produces. The adapter is going to be made from nitralloy and the teeth will be nitrided. So I am concerned that the re-cast layer may produce a brittle layer that when nitrided becomes even more brittle. Is it possible to remove this re-cast layer through hand lapping with a male plug?
I was hoping someone with experience could shed some more light on the issue and possible ways of getting around it.
Thank you