So have a gear thats a interference fit on a shaft. (by 0.08mm)
Both gear and shaft are some sort of nickel - chromium steel simular to en36a (but not necessarily so, detected composition by XRF and found closest match).
There case hardened, but not through hardened. (cutting a old gear is soft inside) But do not know the process used to harden. (suspect carburised, but its a mass produced item from a motorcycle gear box so who knows)
What to try and shrink fit assembly instead of press, But to expand the gear over the shaft would have to heat gear to a calculated 360C. Will this damage the case hardening of the gear? and any ideas as to what max temperture could be used used.