Hello everyone!
So I'm messing around with a concrete floor. I have a point load of 60 kN acting on an area of 0,04 m². I calculated the Winkler coefficient as 9,2 MN/m³. The floor slab is 200 mm thick, C35/45 concrete.
I have a handbook for concrete floors (it's in Estonian, so no point in mentioning the title) so I tried to calculate moments in the slab using formulas from there and also modelled a slab in SCIA Engineer and applied the aforementioned properties to it.
The results are interesting: in SCIA I get a moment of around 12 kNm/m under the load in the slab and using the Westergaard formula from the handbook I get the moment as 2,8 kNm/m. That's a difference of over 4 times. In SCIA I get a bearing pressure of 5 kPa and using the handbook I get a bearing pressure of 157,3 kPa - WTF? I have double checked the units and everything seems to be correct.
Is the Westergaard model so much more different from just a FEM plate on an elastic support that I get so wildly different results or what do you think is the reason?
So I'm messing around with a concrete floor. I have a point load of 60 kN acting on an area of 0,04 m². I calculated the Winkler coefficient as 9,2 MN/m³. The floor slab is 200 mm thick, C35/45 concrete.
I have a handbook for concrete floors (it's in Estonian, so no point in mentioning the title) so I tried to calculate moments in the slab using formulas from there and also modelled a slab in SCIA Engineer and applied the aforementioned properties to it.
The results are interesting: in SCIA I get a moment of around 12 kNm/m under the load in the slab and using the Westergaard formula from the handbook I get the moment as 2,8 kNm/m. That's a difference of over 4 times. In SCIA I get a bearing pressure of 5 kPa and using the handbook I get a bearing pressure of 157,3 kPa - WTF? I have double checked the units and everything seems to be correct.
Is the Westergaard model so much more different from just a FEM plate on an elastic support that I get so wildly different results or what do you think is the reason?