ahmadire, UHA-44 is about limits on post fabrication strain with / without heat treatment for the various materials. You will see that for the austenitics it is applied at design temperatures of 1000 F and up. Referring to Sec II, Part D, Table 1A, SA-240-316L (which is listed in Table UHA-23), maximum design temperature is 850 F, therefore the post fabrication strain limits of UHA-44 do not apply to 316L.
Regards,
Mike
The problem with sloppy work is that the supply FAR EXCEEDS the demand