Why Pressurize an Outside Plant Enclosure

Status
Not open for further replies.

BobkTX

Computer
Nov 30, 2006
1
I am looking into acquiring an outside plant enclosure for a small, low powered piece of telecommunications equipment. I understand that such systems are sometimes placed in an enclosure that is pressurized with Nitrogen.
1)Why would I want to do this?
2)Are there any industry standards that specify the requirements for such an enclosure?
 
Replies continue below

Recommended for you

I was told once that this is done to keep corrosion of the electrical connections to a minimum. The telecom wire connections are very low voltage, can't tolerate any corrosion. Nitrogren is used because it is cheap.

TygerDawg
 
BobkTX,

This would not necessarily cover the requirements to use such an enclosure, but you might find the requirements the enclosure would need to satisfy from the link below. I would think OSHA or a similar state entity (TX means Texas I assume), might be able to further clarify requirements.