Good to see you again,

I have a one doubt why the pipe material do not contain normalized sign(SA 106 Gr.B N)

please reply me
 
Replies continue below

Recommended for you

ramesh349, this pipe is generally not normalized. Refer the specification, SA-106.

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
It can actually be quite difficult sometimes to find SA-106 in normalized condition. If you want a normalized pipe, you're sometimes better off just specifying another grade such as SA-333-6.
 