Hello Code experts,
I am not able to find information on why SA-334 Gr 6 is not permitted for Sec VIII Div 2 applications. I read notes G24 T1 W6 , W12 , W14 of Part II D written against SA-334-6 for clues but I did not find anything substantial. Can some of you who know things help me here.

Thanks for your help
 
It is there in Table 2A, for Section VIII, Division 2, Class 1 construction. Are you specifically asking why it is not in Table 5 for Section VIII, Division 2, Class 2 construction?
 
Likely because no one has asked for it to be added to Table 5.

If you have a need for it, you should ask the Section II Committee to add it.
 
Thanks for your time and reply @TSG4.

I thought SA-334 Gr 6 might not be meeting certain technical requirements for the Section II committee to exclude it from Div 2 , class 2 construction.

Strangely I am not finding any resources on this topic on the internet. Perhaps I should dig more on this topic.

If you or anyone here like to share their knowledge , experience , opinions ( technical or administrative ) , you are all welcome.

Have a great day All.



 