I'm looking for mechanical properties per ASTM standards and have not found 416 to be included in A276-02a. Any one know why or if I'm totally overlooking were it is? I noticed it being referenced in A582A/582M for chemical composition but thats it. If anyone knows were to find it, please let me know.. Thanks in advance
 
Replies continue below

Recommended for you

In answer to the question from the post's title, 416 stainless is not included in ASTM A 276 because it is a free-machining grade, and all of these are standardized in ASTM A 582. The real question is why does ASTM A 582 not include mechanical properties. The answer to that is that free-machining grades can have poor uniformity of properties, and low repeatability from one lot to the next, and these alloys typically are used in non-critical applications, so hardness was determined to be sufficient characterization for this material.

Regards,