The martensitic stainless steels used for premium knife blades are made from a grade which has 15%Cr,0.50%C, 1.0%Mo, and 0.1%V nominally. Does anyone have experience with steel producers who make this alloy?
I believe it can be produced by continuous casting, but I'm not sure. Anyone have a clue?
 
Replies continue below

Recommended for you

You could try a company called Uddeholme. they do make some exotic stainless steels
 