who produces 440B? 1

Status
Not open for further replies.

mcguire

Materials
Joined
Nov 2, 2001
Messages
1,086
Location
US
The martensitic stainless steels used for premium knife blades are made from a grade which has 15%Cr,0.50%C, 1.0%Mo, and 0.1%V nominally. Does anyone have experience with steel producers who make this alloy?
I believe it can be produced by continuous casting, but I'm not sure. Anyone have a clue?
 
You could try a company called Uddeholme. they do make some exotic stainless steels
 