Good morning. I had stamped concrete poured in my back yard almost 1 year ago. I was told to wait at least 2 months before I sealed it to make sure it cured. After 2 months, we had really bad weather (hot, cold, windy) and I was unable to seal it. Now there is white residue and discoloration in the concrete. Is there hope for saving this concrete? Is there a way I could "clean" off the residue so I can seal it? When I hose it down, the original color shows through like new but of course it turns white again after it dries. That dark brown band you see is supposed to be all one color.
Thank you


Thank you