npower0073
Electrical
Dear all. On iste we have a 324 hydrogen cooled generator of GE. During last outage we opened the end shields, GE made the MAGIC inspection and also inspection on the stator. It was found signs of white powder on the end windings. It was all over the end windings where some type of tightening material is used to keep the windings attached.
I have seen some comments on the old thread thread605-148662.
Can you give me some idea for a possible casue? I suspect that the specific tightening material is not the fit for purpose one.
I have seen some comments on the old thread thread605-148662.
Can you give me some idea for a possible casue? I suspect that the specific tightening material is not the fit for purpose one.