Sep 25, 2003 #1 tiroch Mechanical Joined Sep 25, 2003 Messages 3 Location CA I can only locate BS4844 Gr. 3E. What is spec for Grade 3D?
Sep 25, 2003 #2 Carburize Materials Joined Sep 23, 2002 Messages 702 Location US BS 4844 is available from Global Engineering Documents Upvote 0 Downvote