Hi all:

I had done a chemical analysis of a sample that give me this values:

C.....0.69%
Si....0.27%
Mn....0.66%
Cr....0.23%
V.....no more than 0.05%

Does any one know what kind it is.
It cames cold rolled 1 mm thick sheet.

Thanks in advance



Pardal
 
Pardal

This chemistry is very close to a Water Hardeneing Tool Steel Class 131 (AISI W4)except that the Carbon content is under the range for this particular class. W4 spec is 0.8-1.2C. However, since the remainer of the chemistry is withhn range it is going to respond very much like W4 and unless it is some borderline or critical application I would not be hesitant to use it as if it were W4.

Leonard Jesus is the WAY
 
pardal

This chemistry is very close to Water Hardening Tool Steel Class 131 (AISI W4) except that the Carbon content is under the range for this particular class.

W4 spec is 0.8-1.2C. However, since the remainder of te chemistry is within range it is going to respond to heat treatment very much like W4 and unless it is a borderline or critical application, I would not be hesitant to use it as if it were W4.

Leonard Jesus is the WAY
 
Thanks for it.

It seem to be a customer at order made one.

Pardal

Of course
Pardal
 