coulD you tell me about which metals is suitable for pumping coca cola.NI- resist?
Thank you
 
Gorkus:

You don’t state it, and I’ll have to assume you mean fully carbonated Coca-Cola “soda” at a temperature range of approximately 50 – 120 oF.

I haven’t pumped actual Coke, but I’ve successfully pumped a lot of totally carbonated fluids, including water, for many years employing normal meehanite cast iron or 316 stainless steel. I never experienced any corrosion, pitting, or material failure with these materials.
 
Remember that Coke has a lot of phosphoric acid in it

"If A equals success, then the formula is: A = X + Y + Z, X is work. Y is play. Z is keep your mouth shut."
-- by Albert Einstein
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top