Hi,

Does anybody know US suppliers of 316SS piping and flanges (ANSI and DIN flanges) with the European EN 10204 - 3.1B material certification?
 
Note that the european 3.1B certificate used to be specified in accordance with DIN 50049. The EN 10204 standard is adopted from this standard. Just in case, this may ring a bell for a supplier.

Basically it means that the material certificate or mill report shall be issued by the manufacturers (own) independent inspection unit/department)

I would assume that any US supplier who has ever supplied piping components to Europe will be familiar with this type of certificate.

regards
Mogens
 