bulkhandling
Mechanical
HI, How can I get the yield strength of A335 P22 at temperature of 955F? Is the following correct?
30000/20000x11000=16500
Where,
Yield strength at normal temp=30000psi
Allowable stress at normal temp by ASME B31.3=20000psi
Allowable stress at 950F by B31.3=11000psi
My problem is that the pipe expansion loop does not resume the original installation position when it cools down after
normal operation at 955F. Does the calculated stress has to be larger than the yield strength at the deformation points?
Many thanks
30000/20000x11000=16500
Where,
Yield strength at normal temp=30000psi
Allowable stress at normal temp by ASME B31.3=20000psi
Allowable stress at 950F by B31.3=11000psi
My problem is that the pipe expansion loop does not resume the original installation position when it cools down after
normal operation at 955F. Does the calculated stress has to be larger than the yield strength at the deformation points?
Many thanks