Does anyone know where I can get/buy some GLARE material samples for my tests ?
 

Regards, Wil Taylor

Trust - But Verify!

We believe to be true what we prefer to be true.

For those who believe, no proof is required; for those who cannot believe, no proof is possible.
 
Thanks wktaylor , but the wikipeida company name mentioned Cytec does not produce GLARE itself but rather provide the epoxy and resin that is used to produce GLARE :-)

Cheers
 
GLARE is currently produced by Cytec Engineered Materials in Wrexham, UK who supplies it to the Airbus A380 component manufacturing facilities at Stork Fokker in the Netherlands as well as at Airbus in Nordenham, Germany. Stork Fokker has opened a brand new facility next to its existing facilities in Papendrecht, the Netherlands. There Stork Fokker is able to produce Glare sheets of 4.5 x 11.5 m including the milling of doors windows etc. on a state-of-the-art 5-axis milling machine with a movable bed. See attached TDS.

GLARE Configurations
Designation Aluminum Fiber Orientation
GLARE-I 7075-T6 Unidirectional*
GLARE-2 2024-T3 Unidirectional*
GIARE-3 2024-T3 50/50 % Crossply
GLARE-4 2024--T3 70/30 % Crossply

These are places to start "calling".
---------------------------------------------------------
Some interesting tech reports on GLARE ...

OPEN HOLE MULTILAYER FATIGUE CRACK GROWTH IN GLARE UNDER COMBINED TENSION BENDING

WL-TR-94-3134 DAMAGE TOLERANT REPAIR TECHNIQUES FOR PRESSURIZED AIRCRAFT FUSELAGES

AFIT/DS/ENY/97-4 Thickness Effects on a Cracked Aluminum Plate with Composite Patch Repair

AFIT Thesis MECHANICAL PROPERTIES CHARACTERIZATION AND BUSINESS CASE ANALYSIS OF THE FIBER METAL LAMINATE GLARE-3 FOR USE AS A SECONDARY AIRCRAFT STRUCTURE




Regards, Wil Taylor

Trust - But Verify!

We believe to be true what we prefer to be true.

For those who believe, no proof is required; for those who cannot believe, no proof is possible.
 
Thanks a lot Wil Taylor :-), I have already emailed them and I am waiting for their reply to confirm about whether they could provide me with GLARE
 