Oct 21, 1999 #1 an1076 Mechanical Joined Oct 21, 1999 Messages 2 Location US Where can I find the Thermal Conductivity of Concrete? And Linoleum if possible?
Nov 4, 1999 #2 legner Structural Joined Mar 24, 1999 Messages 40 Location US The PCI Design Handbook lists some values. The values vary by unit weight between about 20 and 100 (Btu-in) per (hr)(sq ft of area) per inch thickness. See table 9.1.4 of 5th Edition handbook.<br> Upvote 0 Downvote
The PCI Design Handbook lists some values. The values vary by unit weight between about 20 and 100 (Btu-in) per (hr)(sq ft of area) per inch thickness. See table 9.1.4 of 5th Edition handbook.<br>