Hye everybody, I'm searching for characteristics of steels and aluminiums and more precisely :

YOUNG_MODULUS
POISSON_RATIO
MASS_DENSITY
THERMAL_EXPANSION_COEFFICIENT
STRESS_LIMIT_FOR_TENSION
THERMAL_CONDUCTIVITY
EMISSIVITY

If anybody is able to give me interesting links, he'll help me trully...
 
Try

(requires registration)


And if you can get a hold of them, the ASM handbooks are a reliable source.

If you're looking a proprietary metal, the manufacturers web page most likely has a data sheet.

Failing all that, you can always just do a google web search
 
Ok that's cool I have all I was searching for on the first link
Thank you very much kclim :o)
 