Actually in Aramco standard following in written, so in the light of below requirement from client,heat cycles need to be performed??
12.1.9 Materials of construction (pressure-retaining parts of vessel and non-pressure retaining attachments) shall be tested to verify that their mechanical properties (strength, toughness, creep-resistance, etc.) will be retained, considering all of the following thermal treatments that could affect the material:
a) All heat treatment cycles that will be required for the fabrication of the vessel, including as applicable: normalizing, normalizing and tempering, quenching and tempering, intermediate stress relief (ISR), and final postweld heat treatment (PWHT),
b) Two PWHT cycles to account for future repairs and/or alterations.