Dear all,
A pressure vessel to be designed acc. to the following conditions:
- Design Pressure: 600 psig
- Max Design Temperature: 240 F
- Min Design Temperature: 32 F
- Internal Diameter: 144 in
- Corrosion Allowance: 0.125 in
- Material: SA 516 Gr. 70
- Design Code: ASME BPV, SEC. VIII DIV 1
I select 2.375 in thickness for the elliptical head (After Forming) to satisfy internal pressure design.
Now:
- To satisfy MDT the material shall be Normalized.
- As per UCS-56, Table UCS-56-1 & since the welded joints over 1 1/2 in nominal thickness, PWHT is MANDATORY.
- As per UG-79, The calculated extreme fiber elongation percent exceeds 5%
- As per UCS-79 and since extreme fiber elongation percent exceeds 5%, the head shall be Post Forming Heat Treated (PFHT)
My question is:
Is it practical to apply 3 stages of heat treatment (Normalizing, PFHT and PWHT) for my pressure part?
Thank you all from heart
 
Replies continue below

Recommended for you

You can, or just do two...normalizing and PWHT. PWHT is the same as PFHT.
 
Standard Designation:

BPV Section VIII Div 1

Edition/Addenda:

Para./Fig./Table No:

Subject Description:

Section VIII-1, UCS-79(d)

Date Issued:

03/04/1983

Record Number:

BC82-798

Interpretation Number :

VIII-1-83-105

Question(s) and Reply(ies):

Question: Does heat treatment per UCS-56 satisfy the requirements of UCS-79(d) of Section VIII, Division 1, when the extreme fiber elongation is considerably more than 5% and any of conditions (1) through (5) exist?

Reply: Yes.




 
Standard Designation:

BPV Section VIII Div 1

Edition/Addenda:

Para./Fig./Table No:

Subject Description:

Section VIII, Division 1 (1992 Edition, 1993 Addenda); UCS-79(d)

Date Issued:

03/13/1995

Record Number:

BC94-684

Interpretation Number :

VIII-1-95-50

Question(s) and Reply(ies):

Question (1): A cold formed head has to be heat treated to fulfill the requirements of UCS-79(d) in Section VIII, Division 1. Does the term "heat treated subsequently" mean just after forming and prior to any other operation?

Reply (1): No.

Question (2): If Reply (1) is no, then will PWHT in accordance with UCS-56 satisfy the requirements of UCS-79(d) following welding of the head to the vessel?

Reply (2): Yes.
 