Aug 20, 2008 #1 sk10009 Materials Joined Mar 15, 2006 Messages 55 Location KR I'm currently working in refinery industry. I have had something to see what is the purpose of hydrogen probe installed on pressure vessure. The name of pressure vessels are primary and sponge absorber,lean gas knock out drum,stripper,debuthanizer.
I'm currently working in refinery industry. I have had something to see what is the purpose of hydrogen probe installed on pressure vessure. The name of pressure vessels are primary and sponge absorber,lean gas knock out drum,stripper,debuthanizer.
Aug 21, 2008 #2 dcasto Chemical Joined Jul 7, 2001 Messages 3,570 Location US hydrogen is throughout the refinery and it ends up in the light ends. Hydrogen is not friendly to vessels and they must be checked periodically to see if hydrogen is present and is actively impinging the vessels which may lead to vessels failing. Upvote 0 Downvote
hydrogen is throughout the refinery and it ends up in the light ends. Hydrogen is not friendly to vessels and they must be checked periodically to see if hydrogen is present and is actively impinging the vessels which may lead to vessels failing.