Company wants to have a new undergr. firewatersystem.
Competitors accusing each other about the used resin.
How can we test the used resin of a pipe.
We want it to be epoxy.
Send it to a lab? If yes; whitch lab in W-Europe?
Some help greatly obliged.
Maybe should be more clear about my location.
Should be a lab in Belgium/Netherlands.
Pat, its not the issue about the resin supplier, its more the issue about contractor has used the right resin; but its a very good idea to contact that suppliers.
Thank you very much for your input.
Yaeh, you are right.
We just want to know the contractor has used epoxy and not cheaper, p.e. ortoph. resin.
Certificates are in my opinion useless, the most misused and copied pieces of paper.
Greetings
HDPE pipe what is now underground, degrades very fast, we understand epoxypipe is the best against the hydrocarbons in the soil.
We dont want to use cast iron, what has other disadvantages.
Immerse samples of pipe from the field and pipe known to be epoxy and pipe known to be the suspected inferior resin in the hydrocarbon in question and measure loss of properties of each.
Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
Epoxy resin is thermoset material. By heating it up will not melt. Temperature degradation will start direct from solid state.
So use some fire; if material will soften and start to flow it´s not epoxy.
There are more than one type of thermoset. Also when in a composite it is harder to analysis the resin used. two options are performance based tests or chemical analysis. As these resins tend to be quite chemically resistant, analysis with sophisticated machines is required.
Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
mr. Demon, PVC is really out of the question, it`s not resistent to hydrocarbons, and degrades faster then HDPE.
Saw it on a site here in the neighbourhood.
Also the mechanical properties are a problem.