Jun 17, 2020 #1 Mohammad mehdi Chemical Joined Jun 17, 2020 Messages 1 Location DE Hi What is polypropylene grade of sediment water filter ? Regards https://files.engineering.com/getfile.aspx?folder=cdbfde06-771e-4f5f-a3af-b05f6be2cd34&file=A549ECB9-7D36-4488-BDAB-A0DE0733364F.jpeg
Aug 14, 2020 #2 rd_engineer Automotive Joined Aug 14, 2020 Messages 3 Location PT This PP grade material should be a grade to be injected (low Mw), it must be indicated to support the temperaturas indicated and should be certificated to be in contact with water. Upvote 0 Downvote
This PP grade material should be a grade to be injected (low Mw), it must be indicated to support the temperaturas indicated and should be certificated to be in contact with water.
Aug 30, 2020 #3 Alexandr36484 Chemical Joined Jul 18, 2016 Messages 8 Location UA Hello dear colleagues. Such material is made using spunbond technology. Upvote 0 Downvote