Hi all.
I have been reading and lurking for awhile and nust say that this is a great forum..
I am in the planing-design stage of a hybrid CRD EFI system for retro fit to older IDI diesels. I am mostly doing this for myself, but some others may tag along for the ride.
This will be on a 5.7l GM diesel (yes the olds diesel) but the basic design could be used on 6.2l, 6.5l and 6.5T diesels.
I would expect pressure could be as high as 1600 bar, but I really expect them to be in the 1100-1300 bar range. VW Style TDI injectors will be my choose, with a lot more volume (3x) for the differance in engine size. 5.7l vs 1.9l.
What can I use to make some fuel rails out of. I don't think I need too large a size as a lot of gasoline V8's in excess of 1000hp do not use overly large id bores.
I am going to make adapters to fit the Bosch style injectors to fit the hole in the head. I am looking at using a aftermarket sequential EFI controller, with a crank trigger. Of course no one says the have a diesel system. I have a few issues to work out with that but they do not seem to be mayor issues. Like MAP, TPS, and a couple others...
Thanks
Richard Green
New Ulm, TX
I have been reading and lurking for awhile and nust say that this is a great forum..
I am in the planing-design stage of a hybrid CRD EFI system for retro fit to older IDI diesels. I am mostly doing this for myself, but some others may tag along for the ride.
This will be on a 5.7l GM diesel (yes the olds diesel) but the basic design could be used on 6.2l, 6.5l and 6.5T diesels.
I would expect pressure could be as high as 1600 bar, but I really expect them to be in the 1100-1300 bar range. VW Style TDI injectors will be my choose, with a lot more volume (3x) for the differance in engine size. 5.7l vs 1.9l.
What can I use to make some fuel rails out of. I don't think I need too large a size as a lot of gasoline V8's in excess of 1000hp do not use overly large id bores.
I am going to make adapters to fit the Bosch style injectors to fit the hole in the head. I am looking at using a aftermarket sequential EFI controller, with a crank trigger. Of course no one says the have a diesel system. I have a few issues to work out with that but they do not seem to be mayor issues. Like MAP, TPS, and a couple others...
Thanks
Richard Green