I am designing a small spring clip from stainless and need suggestions on what type of stainless to use. The clip will be about .018-.025 thick, half an inch wide and formed into a hoop with ears/mounting tabs. I'd like a stainless that does not need to be heat treated after forming, will hold it's shape well and be resistant to corrosion. Magnetic properties is not an issue. Any suggestions?