I have been a certified concrete tech for 23 years, I do not carry my card, I have no sticker on my hard hat. You want to know if I,m certified, try internet on the aci page. my names on the list. constuction inspector, have no used for it, company cannot make money with a construction inspector. Thats the job of the engineer, not the testing lab.
What makes a good tech, easy, being able to handle any job without having to have a buddy ride with you. piles, concrete, asphalt, density, undercut. lab work, concrete lab work, writing reports. There are easily 300 different task that need to be known. I, as a senior tech do not have time to hold your hand. what makes a good tech, knowelge and expriences. also when to shut up.