Hi All,
is it correct to say that the thickness range for a WPS goes from 5mm to 50 mm knowing that:
a pqr was performed for each process ( ie: PQR1 with mcaw and thk of coupon is 14mm, the second pqr with fcaw and thk of coupon is 20 mm and the third pqr with saw and thk of coupon is 25 mm)
thank you in advance
is it correct to say that the thickness range for a WPS goes from 5mm to 50 mm knowing that:
a pqr was performed for each process ( ie: PQR1 with mcaw and thk of coupon is 14mm, the second pqr with fcaw and thk of coupon is 20 mm and the third pqr with saw and thk of coupon is 25 mm)
thank you in advance