Aug 6, 2021 #1 sinnatasha33 Materials Joined Aug 6, 2021 Messages 1 Location IN being a wholesaler of inconel 625 flanges I would like to the difference between the two materials of Inconel and Incoloy. http://www.metalloyinternational.com/stainless-steel-304-forged-fittings-manufacturer-supplier.html
being a wholesaler of inconel 625 flanges I would like to the difference between the two materials of Inconel and Incoloy. http://www.metalloyinternational.com/stainless-steel-304-forged-fittings-manufacturer-supplier.html
Aug 19, 2021 #2 BenMacier Mechanical Joined Aug 15, 2021 Messages 68 Location BE Inconel and Incoloy are trademarks. Better use UNS or EN designations to refer to a specific alloy. Upvote 0 Downvote