Jun 18, 2002 #1 scyeunghk Mechanical Joined Jun 14, 2002 Messages 6 Location CN Can anyone tell me about what properties of the surface of AL6061 after anodizing? Besides, what is the difference between hard anodizing and normal one? Just only the difference in the thickness? Is there any web site tell much about these? thanks
Can anyone tell me about what properties of the surface of AL6061 after anodizing? Besides, what is the difference between hard anodizing and normal one? Just only the difference in the thickness? Is there any web site tell much about these? thanks
Jun 18, 2002 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US Check out these two threads on Eng-Tips as well as the links to other websites to which they refer: thread338-23228 thread330-22054 Upvote 0 Downvote
Check out these two threads on Eng-Tips as well as the links to other websites to which they refer: thread338-23228 thread330-22054
Jun 21, 2002 #3 jagad5 Mechanical Joined Jun 21, 2002 Messages 85 Location US Search for papers by Rateick. He has published some papers on this subject including anodize on 6061 in particular. Doug Upvote 0 Downvote
Search for papers by Rateick. He has published some papers on this subject including anodize on 6061 in particular. Doug