Jul 8, 2015 #1 tarekdata Industrial Joined Feb 12, 2007 Messages 20 Location SA Dear API std specialist. According to API 1104 , which pipe thickness tiger " threshold " starting Post welding heat treatment. Thanks Tarek
Dear API std specialist. According to API 1104 , which pipe thickness tiger " threshold " starting Post welding heat treatment. Thanks Tarek
Jul 8, 2015 #2 jte Mechanical Joined Apr 8, 2002 Messages 2,357 Location US Hi Tarek- API 1104 is available at http://www.techstreet.com/api/products/1863960 Perhaps you will consider purchasing the standard which you seem to be using for your engineering or fabrication activities. That way, you will have it available as a ready reference. Upvote 0 Downvote
Hi Tarek- API 1104 is available at http://www.techstreet.com/api/products/1863960 Perhaps you will consider purchasing the standard which you seem to be using for your engineering or fabrication activities. That way, you will have it available as a ready reference.
Jul 9, 2015 #3 LittleInch Petroleum Joined Mar 27, 2013 Messages 22,911 Location GB It's nothing to do with 1104 - it's to do with what the procedure requires which in turn, as a minimum, is what the design code requires. Remember - More details = better answers Also: If you get a response it's polite to respond to it. Upvote 0 Downvote
It's nothing to do with 1104 - it's to do with what the procedure requires which in turn, as a minimum, is what the design code requires. Remember - More details = better answers Also: If you get a response it's polite to respond to it.
Jul 20, 2015 #4 weldstan Materials Joined Jun 24, 2011 Messages 2,805 Location US API 1104 does not provide the info regarding the thickness mandates for PWHT. B31.8 and B31.4 do. Upvote 0 Downvote
Aug 20, 2015 #5 Inspectoriam Petroleum Joined Nov 8, 2013 Messages 5 Location US 1 1/4" is the thickness requireing PWHT within ASME B31.8 Gathering systems, this is the same as ASME B31.4 Upvote 0 Downvote
1 1/4" is the thickness requireing PWHT within ASME B31.8 Gathering systems, this is the same as ASME B31.4