I find in a specification this comment:
All shell and head welds shall clear nozzles and if not possible weld be 100% radigraphed
what is mean clear nozzles ?
 
Replies continue below

Recommended for you

Essentially they do not want a nozzles welded into longitudinal or circumferencal shell/head welds.
 