I just got a CBR of 125 with 12% fly ash added to the soil. Is that even possible?
LL = 50; PL = 12; PI = 38. USCS = CL/CH. We added the fly ash, waited 10 minutes, compacted to target density, waited 2 hours, soaked 4 days and tested.
I was trying to determine the design CBR for when the project gets going. The client wanted 20-25, and estimated we would need to add 15-18% fly ash to get that.
Thanks in advance
M-I-Z
LL = 50; PL = 12; PI = 38. USCS = CL/CH. We added the fly ash, waited 10 minutes, compacted to target density, waited 2 hours, soaked 4 days and tested.
I was trying to determine the design CBR for when the project gets going. The client wanted 20-25, and estimated we would need to add 15-18% fly ash to get that.
Thanks in advance
M-I-Z