Dear Corrosion specialist.

What is the main function of corrosion coupon?
What is the best location and position to be installed?
What is the main types and options for this coupon?
 
Replies continue below

Recommended for you

Flow from well decreased, resulting in low velocity, water collected in low spots instead of being swept along, pitting corrosion begins ... bang. That's exactly why corrosion allowance never helps anything.

OMG%20something%20else.png
 