Hello everyone, a bit of a general question:

Let's say there's an existing above ground pipeline with one small section to be modified. Upon review there is concern that it currently does not meet B31.4 Code, occasional stresses are too high, inadequate supporting, etc. But it's been there 30-40 years in operation, no issues. If there are modifications done, does the entire line then need to be made to comply with the Code? This line has practically zero restraints, so there's not an obvious point to end the calculation.

Line is 16"NPS, A106-B, Std Wall, hoop stress below 20% yield.

Thanks in advance!
 
Not enough information to make a comment.

B31.4 is not the best code for above ground systems and all code will be conservative as will any analysis. Reality is different.

Looks very low stress for pressure so lots available for thermal.
 
What is "required" depends entirely on the owner's requirements and any applicable regulations. In general, you don't have to go back and bring the line up to meet current code requirements, but you do need to determine if any of the issues you have identified are fitness for service issues.

Pipelines in operation often no longer meet the original design code for many reasons (e.g., corrosion) but can still be fit for service. It's hard to comment on your situation without more detail.
 
How far you need to model is not fixed. If no clear anchor or line stop then I would go at least 200m from your modification.

Might be a bit excessive, but when you make changes, you get blamed for anything happening even if the fault or overstress is already there.

So model it now in its as Installed condition and don't make anything worse with your changes.
 
But it's been there 30-40 years in operation
Probably the pipeline has outlived its design life. If so, the remaining life with respect to corrosion etc. should be investigated and suitable replacements as required should be made.
 
Thank you to everyone for your input. Have a meeting this week with Owner to discuss options.
 
Hello everyone, a bit of a general question:

Let's say there's an existing above ground pipeline with one small section to be modified. Upon review there is concern that it currently does not meet B31.4 Code, occasional stresses are too high, inadequate supporting, etc. But it's been there 30-40 years in operation, no issues. If there are modifications done, does the entire line then need to be made to comply with the Code? This line has practically zero restraints, so there's not an obvious point to end the calculation.

Line is 16"NPS, A106-B, Std Wall, hoop stress below 20% yield.

Thanks in advance!
when you say, "upon review" and make a statement that it 'doesn't meet B31.4 code', you much have studied the stress report in detail. Don't you have the stress model or is your statement based on the report only?
Typically, the Code wants that the piping system should be taken as a whole when calculating the flexibility of the system.
The Code also tells that you don't have to do a formal flexibility analysis if there is no significant modifications and if the system had successful operating record (which you have).
 
You state that the pipe line is at a hoop stress < 20% of the SMYS. How can you truly overstress such a line unless it as hit by a truck or a 7 plus seismic event?
 
He says it fails occasional stresses, so I'm guessing that because it is not adequately anchored, when you model the line, the wind and/or seismic cases cause gross displacement of the line resulting in overstress.

"Inadequate support" may also mean that spans are too long and you're getting high stresses at support points.
 