WHAT IS THE EQUIVALENT ASME MATERIAL FOR EN 10222-5?
 
A materail equivalency book is either published by SAE or ASTM. If its available on a CD it could make for an easier search. I think it's called unifying material identification system or something of the like. GOOD Luck.
 