Dear Engineers
Our company is EPC contractor of for Gas Compressor Stations that Des. Press.=1436 Psi and Des. Temp.=-15/83 C .
Oue design for material of Ball Valve Bodies were A350 LF2 but MC company chenged the material to A350 LF6 CL.2 .At first What I'm looking for is the difference between these two grades of A350 and then ,is it possible to use A350 LF2 or not ? because as you know the price for A350 LF6 CL.2 is more expensive than LF2 (about 20%).
Thanks
Our company is EPC contractor of for Gas Compressor Stations that Des. Press.=1436 Psi and Des. Temp.=-15/83 C .
Oue design for material of Ball Valve Bodies were A350 LF2 but MC company chenged the material to A350 LF6 CL.2 .At first What I'm looking for is the difference between these two grades of A350 and then ,is it possible to use A350 LF2 or not ? because as you know the price for A350 LF6 CL.2 is more expensive than LF2 (about 20%).
Thanks