Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

what is the best way to weld a stee 1

Status
Not open for further replies.

Chamberlin

Mechanical
Jul 2, 2001
14
what is the best way to weld a steel tube spout 20mm dia into a hole on a mild steel pressing thk 1.25mm, This operation is required to be repetative 10000/day
 
Replies continue below

Recommended for you

The fastest way is projection welding if the parts can be made to accomodate the process. That will require that the tube have an area that can be displaced down onto the other part. This provides the filler material for the weld.
If the part can't be made in a way that allows this you are probably looking at robotic MIG welding.

Steve
 
Thanks Steve I think projection welding may be the way to go, Where can I find more about the process, These are small repetition pressed parts can you help further?