What's preferable for a steel worker to place; 3/16" or 1/4" fillet weld?
We're attaching auxiliary steel to existing building steel to support some lightweight pipe (<1 kip at most support points). For our application either size is sufficient as 3/16" fillet weld provides 4.2 kips/in strength capacity for longitudinally loaded weld and 6.3 kips/in for transversely loaded weld.
We're attaching auxiliary steel to existing building steel to support some lightweight pipe (<1 kip at most support points). For our application either size is sufficient as 3/16" fillet weld provides 4.2 kips/in strength capacity for longitudinally loaded weld and 6.3 kips/in for transversely loaded weld.