Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

What is KE672 tool steel? 1

Status
Not open for further replies.

RPstress

Aerospace
Joined
Jun 4, 2003
Messages
846
Location
GB
This may be an older UK spec. It's listed by some suppliers, but I can't find any composition or hardness, etc.

Can anyone help?
 
If I remember correctly, KE stood for Kaiser Ellison - They were a Sheffield (UK) company who made specialist steels.

An old catalogue I have shows:

KE 672 is (was) a Non-Shrinking Oil Hardening Tool steel to BS 4659:1971:BO1

Composition:
0.85-1.00 % Carbon
0.4% max Silicon
1.10-1.35 % Manganese
0.4-0.6% Chromium
0.4-0.6 % Tungsten
0.25% max Vanadium

Used for press tolls, knives, punches, dies gauges, moulds etc.

 
Thanks, geoffthehammer. That's exactly what I needed.